Kitchen Worktop


Author
Message
surferx
surferx
Supreme Being (81 reputation)Supreme Being (81 reputation)Supreme Being (81 reputation)Supreme Being (81 reputation)Supreme Being (81 reputation)Supreme Being (81 reputation)Supreme Being (81 reputation)Supreme Being (81 reputation)Supreme Being (81 reputation)
Group: Forum Members
Posts: 8, Visits: 60
I would like to cover the Kitchen Worktop, in my camper with a single layer of carbon cloth and hi temp laminating reason.

I was intending to use

Carbon Fibre 2/2 Twill 3k 199g

Very High Temperature Epoxy Laminating Resin 500g Pack

I have done a few structural repairs with carbon before but that is it, so I understand how to lay the fibre and resin, but I am looking for advice or a guide on how to get a flat gloss finish, ideally a mirror like one.
Reply
surferx
surferx
Supreme Being (81 reputation)Supreme Being (81 reputation)Supreme Being (81 reputation)Supreme Being (81 reputation)Supreme Being (81 reputation)Supreme Being (81 reputation)Supreme Being (81 reputation)Supreme Being (81 reputation)Supreme Being (81 reputation)
Group: Forum Members
Posts: 8, Visits: 60
Would you recommend that I put anything over the resin, glass, plastic? Or just leave to cure?

thanks for the advice so far!
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search