Hello everybody,
I'm new on this business, so I hope you can help me with this issue.
I want to make some dashboard's parts (23x18x1.5 cm) with carbon fiber laminating kit. However, these parts seem to be a little complicated to make a mould first, and then the carbon fiber part. I think there wouldn't be problem any problem with the front of the part (see picture). 

http://www.talkcomposites.com/Uploads/Images/89dce4c8-afed-4063-97ed-5630.jpg


But I see some difficulties with the back of the part due to flanges, ribs or threads (see picture) where screws make this part fit in the dashboard.

http://www.talkcomposites.com/Uploads/Images/be0381c3-b3bc-499f-8c48-73af.jpg            http://www.talkcomposites.com/Uploads/Images/85090a78-c93f-439a-a8bf-72a1.jpg


I was thinking in making a mould of the front and then make the front with carbon fiber. Then make a mould of the back and then make the back with resin only, since I see a bit difficult to use carbon fiber or glass fiber to make the back. The problem would be to join both parts together and get the right thickness of the original part. Fail to do this will mean noise because of vibration and also part wouldn't fit in dashboard properly.

Do you have any advice to make this part properly? Have you ever made a similar part like this?
Do you know if it's possible to mix carbon fiber and glass fiber in order to get the required thickness?
Do you know the right technique to make this part and similar ones?

I would really appreciate your answers.

Thanks.
Replies
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
The simple answer is that it can't really be done. 

Those parts are made via plastic injection moulding, a technique which is totally different to composite moulding. The only way to do it with composites is to mould the front, and produce that in carbon. Then you need to get creative with your fasteners on the back. I generally use nutserts for threaded fasteners, and fold up some aly flat bar for any tabs etc. Clips and the likes are not your friend, they don't work with composites. The easiest solution is 3M dual lock velcro. 

To be honest, yours looks relatively simple compared to others I have seen. Bond in some nutserts and get some 3M dual lock velcro and you're away. 
Edited 10 Years Ago by Hanaldo
Inkatreker
Inkatreker
Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)
Group: Forum Members
Posts: 5, Visits: 43
That's a good piece of advice Hanaldo. Thanks.
Any recommendation to stick nutserts, fasteners and tabs to the back of the carbon fiber? I mean, should I use any kind of glue or resin?

Thanks.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search