TomBombRiot
TomBombRiot
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 2,
Visits: 11
Hi,
I am new to the whole mould making process, so I need to get some info to quickly get me started.
My main question is - is it possible to use a material (e.g. HDPU foam), CNC mill an inverted female (cavity) mould, coat it with resin and use this as the female mould to put prepreg carbon fiber in and cure in oven?
It would make the mould making so much easier compared to having to do a model and then make a glass fiber mould from it.
Very thankful for input on this
/Thomas
Edited
11 Years Ago by
TomBombRiot
Reply
Like
2
Hanaldo
Hanaldo
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Yep, totally fine. Composite company here in Perth is currently building the southern hemispheres largest carbon fibre catamaran, and they are doing it using CNC'd foam as a mould.
Just one thing to think about, the moulds won't last long. For low production runs they are ok, but don't plane to get 50 parts out of one.
Reply
Like
3
TomBombRiot
TomBombRiot
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2,
Visits: 11
Great, thanks!
Reply
Like
3
Matthieu Libeert
Matthieu Libeert
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
make sure your HDPE PU is resistent till the temperatures used for prepreg, as well as your coating resin
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
3
kidpaint
kidpaint
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 99,
Visits: 676
We just got some plugs in today that were cnc machined from foam. Im not sure what type of foam is is though. We are using PE resin to make the molds
Reply
Like
3
VVS
VVS
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Moderators
Posts: 226,
Visits: 334
So what kind of finish would you get in/on the resin from this technique.
would there be much work needed before you could lay your part?
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search