Hello all,

Can anyone tell how I can eliminate the voids I get aroundthe edges/corners of my foamcore during a vacuum bag lay up?  My layup is a lamination of fiberglass, wood, foam core & carbon fiber. I believe my all my layers are wetted outcompletely before they are placed on the mold. I use a peel ply & bleedermaterial before putting on the bagging film. Attached is picture one of the problemareas.

TIA,

Paul


Attachments
badvac.PNG (524 views, 2.00 MB)
Reply
grafgulch
grafgulch
Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)
Group: Forum Members
Posts: 4, Visits: 63
Thanks.. I will try that.
 I know sometimes my bagging film is pulled kind of tight. I do use a very thin bagging film with lots of stretch. Visually, the bagging film looks like to conforming to all the inside corners very well.

I guess my next question is: Whats the best way to fix these voids? normally my next step is to apply 2 layers of very lightweight cloth (1.45 oz deck cloth) with the vacuum bag applied directly to the part (with bleeder material on the side) to produce a smooth glossy finish. If I  use lots of pleats on the next step I am afraid I won't  get a smooth finish.

 I am thinking I need to fix these voids before the next step, otherwise I won't get the nice smooth finish at these problem areas. 

Paul  
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search