Hi all, I have done some carbon wet lay in the past with good success. Have decided to try the uni mould and have stumbled across a problem - the gel coat started curing during application and went lumpy before I realised and had brushed on an area. I didn't have time to smooth the rest out eithwr as it would have curdled too ! Is this done for or can I just apply second goat as normal once tacky ? In other words is this going to show through and effect the final mould ?

See picture below to see what I mean !

Many thanks
Attachments
20150408_194544.jpg (467 views, 4.00 MB)
Edited 10 Years Ago by James91h
Reply
VVS
VVS
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Moderators
Posts: 226, Visits: 334
Hi James.

Ive just done my first mould with the uni system and although I didn't suffer your problem I was close and the last bit of resin that I didn't use was lumpy.

All I can say is don't use a tall narrow pot to mix, one with a similar hight to width is best.

Get it out of the pot and onto the plug asap and you will find its workable for much longer.




When you move onto the next steps be very organised, cut all your matt ready, mix small amounts of resin, I found 500gram to be the max I could work and again work quickly and get the resin onto the job.

If you don't cut your matt before starting you will have problems as once started you need to keep flowing.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
James91h - 10 Years Ago
The Fibreglass King - 10 Years Ago
James91h - 10 Years Ago
panda - 10 Years Ago
Hanaldo - 10 Years Ago
James91h - 10 Years Ago
The Fibreglass King - 10 Years Ago
VVS - 10 Years Ago
James91h - 10 Years Ago
Hanaldo - 10 Years Ago
VVS - 10 Years Ago
Hanaldo - 10 Years Ago
VVS - 10 Years Ago
Hanaldo - 10 Years Ago
James91h - 10 Years Ago
Hanaldo - 10 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search