Epoxy Mould Making Putty


Author
Message
scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
Hi there, I couldnt find any info on the TDS and the tech questions about the epocy putty.

Im going to make a couple of car mirror moulds as they are nice and small, my main question is does the putty need to be post cured at all? and if so how much?
The other question is what temperature can they go to, can a low temp cure prepreg be used in them?

Thanks
Gaz
Reply
scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
Hi warren, thanks for the info. will try and get an order in today or next week.

interesting to know dravis, I thought the epoxy might be able to handle something a bit higher, If i can use the easy preg at 80degrees then that could be ok.

I can cope with wet lay + vacuum bags for now as Im hoping to machine some ali tooling in the future once i have some cash.