Hi there, I couldnt find any info on the TDS and the tech questions about the epocy putty.

Im going to make a couple of car mirror moulds as they are nice and small, my main question is does the putty need to be post cured at all? and if so how much?
The other question is what temperature can they go to, can a low temp cure prepreg be used in them?

Thanks
Gaz
Reply
Dravis
Dravis
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
only 60 degrees .. WowWhistling   I've used it a lot, and postcured parts in "putty" moulds up to 100 deg ... Never gave it a second thought--- its Epoxy, most epoxies easily handles 100 degrees..

.. OK ... 120 degree or more Prepreg ... probably not ... but my experience tells me thet the putty does not distort noticably at 100 .. for small thick moulds...

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search