Total weight of resin and carbon cloth


Author
Message
CurlyHutty
CurlyHutty
Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)
Group: Forum Members
Posts: 2, Visits: 5
Hi - I have searched for the answer to this - to no avail.  I would have thought it was an FAQ ...

Are there any rules of thumb to estimate the total weight of a carbon-fibre layup i.e. the weight of the carbon cloth plus the resin?

E.g:
1 layer of 200sgm CF including wet-lay epoxy = XX gsm
2 layers of 200sgm CF including wet-lay epoxy = YY gsm
3 layers of 200sgm CF including wet-lay epoxy = ZZ gsm

Is there a 'standard' ratio of CF to resin?

I only plan to make flat sheets, wet-lay, not infusion, but with pressure to squeeze out as much epoxy as possible.

I am planning to make some aero parts so weight is important.

Thanks!  CH
Reply
CurlyHutty
CurlyHutty
Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)
Group: Forum Members
Posts: 2, Visits: 5
Brilliant - thanks folks.