Adding pigments to organic amines


Author
Message
jayeshrchinchole
jayeshrchinchole
Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)
Group: Awaiting Activation
Posts: 1, Visits: 4
Can anyone suggest an amine stable pigment brand? All the pigments currently are dispersed in epoxies.
Hence, mixing the epoxy dispersed pigments in amine will cause a reaction. I need to colour the amine with pigments.
VVS
VVS
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Moderators
Posts: 226, Visits: 334
I'm not up on resins so have no idea what amines are but I do work for a pigments manufacturers so may be able to help from that side.

I would think you could use some of the metal oxides as these are quite stable as a finished pigment and have good light and heat resistance.

problem is some are controlled regarding what you are allowed to use them in so you would have to have a read up.

Iron oxide may work but colours are limited, you can get a black.

other problems will be mixing/wetting the pigment as epoxy manufacturers will use sheer mixers to thoroughly mix the pigment, you could try a long period of wetting between mixing.

Because I'm not clear on the Amine id say a test sample will be a definite.