carbon fiber finish clear coat?
carbon fiber finish clear coat?
Post Reply
Like
8
carbon fiber finish clear coat?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
TomDesign
TomDesign
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
Hello guys used many things, but found Basco clear products any experience with these? what you use for carbon stuff i mean clear coat so surface become hard as a rock and clear like a glass.
Reply
Like
8
ChrisR
ChrisR
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 363,
Visits: 3K
One of the best I've seen is durepox clear
http://www.marineware.com/durepox-
nigh on impossible to scratch (or sand/finish) after a few days
Reply
Like
7
TomDesign
TomDesign
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
just emailed ye i hope so that do not need heating as marines surface very hard to scratch
Reply
Like
7
JustJDee
JustJDee
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 13,
Visits: 153
We've used an automotive 2pak clear coat, sprayed properly and cured at a low temperature it can provide the finish you're after. However it is pretty hard to get a perfect finish for a rookie spray painter!
Reply
Like
7
TomDesign
TomDesign
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
Man i do overlay for Lamborghini, Ferrari and so on. im trying to find perfect clear coat. as if i polish resin it is not protected fro uv.
Reply
Like
7
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
8
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search