I am working on the design of an impact attenuator for a Formula Student car. 

I am interested in using aluminium honeycomb, specifically the 19.1mm cell size as it is the most cost effective, and I am in the process of testing a design using this in solidworks. 

One concern I have is how the sheets and honeycomb layers will be bonded together. 

I have attatched an image of the current attenuator design because it is a little bit difficult to explain. 

I would like to know, along with what the best resin/adhesive to use is, what material exactly should be selected and used during the cad process. 

I can see that it is of the 3003 series, however I am unsure what material out of this series specifically as they are given properties in solid form rather than treated as a honeycomb section.

All help and feedback is greatly appreciated!

I am also open to using a different material providing it is not ridiculously expensive. The budget for this project is around £500 so it is limited.









Attachments
att screenshot.png (758 views, 150.00 KB)
att screenshot2.jpg (877 views, 59.00 KB)
Reply
NigelGroom
NigelGroom
Supreme Being (166 reputation)Supreme Being (166 reputation)Supreme Being (166 reputation)Supreme Being (166 reputation)Supreme Being (166 reputation)Supreme Being (166 reputation)Supreme Being (166 reputation)Supreme Being (166 reputation)Supreme Being (166 reputation)
Group: Forum Members
Posts: 10, Visits: 43
Oh right I wasn't aware of that but I shall look into it, thanks. 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search