hi all,

I have a turntable project which I intend to coat with the epoxy coating resin. 

It's made of stacked ply but the primed then painted with a synthetic acrylic rattle can. I'll leave the paint to cure for a week before attempting this.

My question is how do I apply the coating resin e.g. Brush? Roller etc?

Do I need to key the paint surface?

And how do I go about coating the sides without the resin running off?



Thank you in advance, Gavin 
Reply
Mudchute
Mudchute
Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)
Group: Forum Members
Posts: 2, Visits: 8
Here's the piece to be coated.