Gelcoat didn't cure problem


Author
Message
Matthieu Libeert
Matthieu Libeert
Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
hi guys,

So I had a little problem...
The first layer of gelcoat (toplayer) didn't cure I guess...



I was able to safe the part by sanding it of; giving me this result

http://www.talkcomposites.com/Uploads/Images/11b9ea32-9376-48a9-b3b1-27f3.JPGhttp://www.talkcomposites.com/Uploads/Images/f8e337b8-9cd4-449f-808e-3cad.JPGhttp://www.talkcomposites.com/Uploads/Images/70dbf301-d3e2-4acc-875c-d3b6.JPG


So whats next:

-I will clean the mould, any of you have an idea how I could do this the easiest and best way?
-Sand the part with sandpaper grid 80
-Apply gelcoat in the mould ,then add a new toplayer of carbonfiber, add some resin, put the part back and vacuumbag it all again for 24h

any more advice?  

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search