I've been asked to fix a friends boat where some self tappers have pulled out over time.  I have access from 1 side only so no bigheads I'm afraid.  Its 10mm thick GRP.  Can I use a helicoil in it?  Or should I thread it out to M12 and bond in an M12 piece with an M5 tapped hole down the centre?  Is there anything else I can do?
Reply
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
How much of a load is being applied? There's a few options available but would have thought a bonded insert would work