hi

i am kind in process of learning and doing stuff. so not all the materials and all the equipment in the house Smile
so i'am trying to improvise and find solution from existing materials and tools that i have.

i'am planing to do mould, but i dont have gelcoat.

so will thickened resin with fumed silica do the job instead of gelcoat.
i am talking about the mould for just a couple of uses.
dbcrx
dbcrx
Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)
Group: Forum Members
Posts: 46, Visits: 1.2K
yes, thats basically what gel coat is anyway. if you have any colour pigment that will help to see what your doing when sanding/polishing.
tomzi1234
tomzi1234
Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)
Group: Forum Members
Posts: 40, Visits: 500
thank you for your
yes i have pigment. and i am planning to use it. or i will use two. one for each side of split mould. to easily separate them when i will be doing split mould from original object.

another question.
i have read that first couple of releases it is good to use PVA.
so any suggestion what release agent should i use.
carbonfibreworks
carbonfibreworks
Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
Hi Tomzi
This will give excellent results https://www.easycomposites.co.uk/easylease-chemical-release-agent
Chris
Carbon fibre works ltd

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
One thing to remember is that gelcoats are formulated to remain tacky until the backing layers are applied, giving a strong chemical bond between the gelcoat and the backing resin. If you just use thickened laminating resin to make your own gelcoat it will cure hard with a waxy surface if left too long. This will prevent the backing layers bonding properly. Just let it cure to a tack before applying the backing layers and you should be ok.

Carbon Copies Ltd
brainfart
brainfart
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 198, Visits: 1.4K
wozza (30/12/2014)
One thing to remember is that gelcoats are formulated to remain tacky until the backing layers are applied, giving a strong chemical bond between the gelcoat and the backing resin. If you just use thickened laminating resin to make your own gelcoat it will cure hard with a waxy surface if left too long. This will prevent the backing layers bonding properly. Just let it cure to a tack before applying the backing layers and you should be ok.


It depends on what kind of resin you will use, for polyesters: what wozza said, if you use epoxy then that's not an issue since they don't contain the wax additive.
tomzi1234
tomzi1234
Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)
Group: Forum Members
Posts: 40, Visits: 500
thank you all for reply

i use epoxy
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search