Hi Ray,
Brian is right, at -0.8bar you won't quite reach the point where the entraped air does an 'exponential expansion' the closer you get to absolute vacuum the better. -0.8bar will still help to degass... you would just have to wait much longer for the air to rise and burst in a slightly more 'natural' way. If you have any questions on how to get the most out of your equipment/setup just let me know.