is the IN2 epoxy infusion resin UV stable or do parts need any extra protection from a UV clear coat?
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
No such thing as a UV stable epoxy, that's just their nature. Some have stabilisers added to increase resistance, but it's a question of time. All epoxies will degrade with UV exposure unless they are protected. 