IN2 resin UV stable?
IN2 resin UV stable?
Post Reply
Like
4
IN2 resin UV stable?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Bonobo
Bonobo
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 85,
Visits: 1.2K
is the IN2 epoxy infusion resin UV stable or do parts need any extra protection from a UV clear coat?
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
IN2 resin UV stable?
Bonobo
-
11 Years Ago
No such thing as a UV stable epoxy, that's just their nature. Some have stabilisers added to...
Hanaldo
-
11 Years Ago
OK Thanks, so infused parts that will be outside need to be clear coated. or use an in mould...
Bonobo
-
11 Years Ago
IN2 is highly UV resistant for an epoxy but as Hanaldo says. no epoxy is UV proof. If you need...
Warren (Staff)
-
11 Years Ago
Post Reply
Like
4
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search