UniMould Gelcoat dont cure


Author
Message
Dokomo
Dokomo
Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)
Group: Forum Members
Posts: 5, Visits: 30
Hi to all. 

It's my first mould using UniMould system. I follow exactly the tutorials and indications for making the mould. 

For the first step, i have bougth locally an MEKP catalyst ( i have attached the image ). I have applied a thin layer of gelcoat, and 4 hours later, another layer. After that, i have wait to the next day to let it cure, but the surprise was, that the part was totally ruined when i arrived next morning ( i have attached another image ). At that time, it had been drying for about 15h.

The gelcoat has reacted with my part ( a motorcycle fuel tank ), producing great wrinkes all around the part. The tank was just finished, laquered and polished with PPG clear coat, and it has been drying for a week before I apply the gelcoat.

The room temperature was about 17º in the day, and about 13º overnight. 

I have made a test yesterday, using 3 small mixes, one in 2%, another in 5% and a extreme one at 10%. The 2% mix, seems to never cure, it has been applied for about 20h right now, and keeps almost fresh. 5% looks nice, it's tacky in the surface and cured in the inside part, and the 10% mix its fully cured.

I think the problem has been that the mixture at 2%, has react because it has been applied over the clear coat too much time without cure ( i look at it 6h after the application and it has no wrinkles at all ), producing the wrinkles at the end.

The question is, it's safe to work at 5% ? Do you think that the problem it's another one ?

Thanks in advance, and sorry about my english. 
Attachments
IMG_20141118_123600.jpg (759 views, 82.00 KB)
IMG_20141118_132727.jpg (730 views, 34.00 KB)
Replies
Dravis
Dravis
Supreme Being (5.2K reputation)Supreme Being (5.2K reputation)Supreme Being (5.2K reputation)Supreme Being (5.2K reputation)Supreme Being (5.2K reputation)Supreme Being (5.2K reputation)Supreme Being (5.2K reputation)Supreme Being (5.2K reputation)Supreme Being (5.2K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
MEKP is mots often diluted/thinned with something called  Dimethyl phatalate, since concentrated MEKP is an explosive ...Whistling
The locally available MEKP you have is probably diluted much more than the ones Easy Composites normallly use.
Different countries seem to have different laws regarding "deactivating" explosives.

That will almost certainly mean other percentages than "normal" MEKP when added to polyesters as a catalyst.

I think you should try to find out the correct percentage of YOUR catalyst to the "standard Polyesters" that are available locally.

Your "local" MEKP could easily be diluted 5 times more than "standard"

That being said:  17 degrees C. and 13 deg. C.  at night is NOT enough for a proper cure of the EC Unimould system ... You need to have 18 -20 degrees as a minimum.


Perfect example of "alligatoring" in that picture b.t.v.  Crying Pinch SickCrazy

I'm pretty sure your "plug" needs a better coating and thicker waxing ... NO rattle can stuff, only 2- component paint, and still weeks curing at temps lower than 20 deg.

Good luck!!


"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
Edited 12 Years Ago by Dravis
Dokomo
Dokomo
Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)
Group: Forum Members
Posts: 5, Visits: 30
Dravis (20/11/2014)
Your MEKP is diluted/thinned with something that I can not read what is ... Phatalate-something ... Unsure

That will almost certainly mean other percentages than "normal" MEKP
I think you should try to find out the correct percentage of YOUR catalyst to the "normal Polyesters" that are available locally.

Perfect example of "alligatoring" in that picture b.t.v.  Crying Pinch SickCrazy


My MKEP it's diluted with phthalate, i've seen the composition in the specs of the MEKP that sells in easycomposites website, and seems to be the same.

Today it's a little hotter than yesterday, near 21ºC inside the factory, and seems to have a big impact in the curing times too.

Now i have to repaint, re-sand, re-do all the fuel tank and prepare it again for apply the gelcoat .... Pinch
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Dokomo - 12 Years Ago
thorstengsxr - 12 Years Ago
Shaneer22 - 12 Years Ago
Dravis - 12 Years Ago
Dokomo - 12 Years Ago
Warren (Staff) - 12 Years Ago
Dokomo - 12 Years Ago
Dokomo - 12 Years Ago
brainfart - 12 Years Ago
Dokomo - 12 Years Ago
matthieutje65 - 12 Years Ago
Dravis - 12 Years Ago
Matt (Staff) - 12 Years Ago