buy a length of stainless steel thin walled pipe the same diameter as the outside of the tube you want to make.
Get someone with a tube bender to bend it to the correct shape... Polish and wax ...
make a mold from it ... split along the length ... A strong mold ...
Lay up inside .. use a bicycle inner tube to compress the layup from the inside ...
You can even thread CF braided hose onto the tube, for added convenience ..
Good luck ..