From the description it sounds like the use of single tows wrapped around the joint for reinforcing purposes. The technique for that would be the same as wrapping any tape around a joint.
That method is one of several to join tubes. methods include inserts/ferrules either in composites or aluminium, wrapping with tape, using interference fit tubes and bonded at the overlap are just the obvious ones that come to mind.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|