John Hainsworth
John Hainsworth
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 3,
Visits: 11
Is your resin water based allowing it to be mixed with copper powder and used as antifouling on a fibreglass boat?
Reply
Like
3
Reply
John Hainsworth
John Hainsworth
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 3,
Visits: 11
Thanks for the info. My last attempt at coating was a 1/1 mix of epoxy and copper powder which has lasted 5 years and now needs touching up and burnishing. I think I'll go for a stronger copper mix this time and keep it well burnished.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
antifoul
John Hainsworth
-
11 Years Ago
I think the short answer is NO... All the EC stuff are Epoxy or Polyester resins .. But the EC staff...
Dravis
-
11 Years Ago
I want to create my own antifouling mix using epoxy resin and copper powder. Could you recommend a...
John Hainsworth
-
11 Years Ago
Some of the commercial copper antifouling manufacturers claim to use "low solids water based epoxy...
brainfart
-
11 Years Ago
Thanks for the info. My last attempt at coating was a 1/1 mix of epoxy and copper powder which has...
John Hainsworth
-
11 Years Ago
Copperbot (which is now called coppercoat) is said to be 80% copper, too.
brainfart
-
11 Years Ago
As already said, our resins are not really designed to be watered down. Most resins will take a high...
Warren (Staff)
-
11 Years Ago
Old wooden sailing ships used to be "plated" with thin copper plates, nailed to the hull, to sail in...
Dravis
-
11 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search