Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - Product Specific Pages
»
Pre-Preg Carbon Fibre
»
Multiple lines on vacuum pump + scalability
Multiple lines on vacuum pump + scalability
Post Reply
Like
4
Multiple lines on vacuum pump + scalability
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
JCCR
JCCR
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 4,
Visits: 39
Hello guys,
Greetings from Costa Rica! For the past few months I have been working on the design and fabrication of an automotive alignment tool. After analyzing countless ways of making it out of aluminum I have now concluded that the weight, strength and design advantages from making it out of CF are worth the switch. I have been reading your prepreg guides and watched the complex parts video and it looks like a real possibility to make something very nice at a very similar cost so I'm very excited.
My question is the following. Given the vacuum pump included in the starter kit, would it be possible to divide the vacuum line into 4 leads for separate parts or is it necessary to have a more powerful one? The parts are 500 mm x 150 mm x 30mm (hollow) so it looks like 4 can fit into an
Oven
I've looked at but not sure about the vacuum pressure requirements.
Also, how scalable is the process described in your prepreg starter kit? Would it be a problem if vacuum bagged parts are stored in the freezer (or anywhere appropriate) while a 20 unit batches are prepared to cure them all at the same time?
Thanks,
JC
Reply
Like
4
ajb100
ajb100
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 346,
Visits: 4.4K
One pump would be sufficient depending on size of the parts. One pump would be able to pull a full vacuum, but it will take longer than a higher volume pump
Reply
Like
2
Warren (Staff)
Warren (Staff)
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8K
As long as your bags are pretty leak free then you will be fine. We put multiple parts in the oven connected to one pump on a regular basis.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
4
JCCR
JCCR
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 4,
Visits: 39
Ok thanks that's good news then
How much time does one have after laying up the prepreg in the mould to put it in the oven? Can it go back in the freezer/cool area to extend this time?
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
4
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search