I use that gelcoat. I have found that I need to use 10-12 coats of easylease to get a good release (things fall out of moulds at this level). If I use the 6 coats as recomended on the can things stick quite badly.
Could it be that at 5 coats you dont quite have a sufficient coverage so that the gel has found a patch it can stick to whereas the laminating resin found a fully covered area of the mould?
|