Galvanic reaction Carbon on Aluminum how to prevent question


Author
Message
JaWillis
JaWillis
Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)
Group: Forum Members
Posts: 8, Visits: 24
Any input on this would be appreciated

Maybe you can help me. I will be extending a piece of aluminum tubing by first cutting the tubing then inserting a carbon fiber "ferrule" if you will, to extend the tubing. I will then wrap the splice with carbon fiber tape and resin. 

1. What adhesive can I use at the insertion point to bond the aluminum tubing to the ferrule? Will it there be a galvanic response?
2. What do I put in between the carbon fiber wrap and the Aluminum to prevent galvanization?

My third question is how to adhere your prefab carbon tubing to pre-preg carbon fiber? Example: a 42mm ID tubing which happens to be the exact size id of a bicycle Bottom Bracket PF30. (press fit 30). However I need to beef up the wall thickness by wrapping pre-preg around it, then compress and heat to cure. I am concerned there may be a delamination issue between the tubing and the pre-preg. Is there something I need to treat the tubing with prior to applying pre-preg? 

Thanks in advance for your help.

Jim W
Reply
AHA
AHA
Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)
Group: Forum Members
Posts: 6, Visits: 14
We use to smear all alu and titanium parts where it came into contact with the carbon with  two part rubber sealant. It works a treat. 