Group: Forum Members
Posts: 592,
Visits: 1.9K
|
I have just infused a test sheet using ordinary thin (3 mm) floor "anti-sound" cork sheet... not very uniform in thickness, and a bit porous, but very cheap.
I will test it in a few days, when fully cured.
1 layer of 375 gsm Satin weave CF + 1 layer 200 gsm twill on both sides.
I did three strips: 1 floor-cork, 1 Soric and 1 3D-core All 3 mm.