Hi again. I use GC50 gelcoat for all our products. We are new in using this product, I'm having hazy clear coats after a week or two of exposing it to sunlight. At brand new condition there are no problems. I sprayed the GC50 with gelcoat spraying gun. Single layer. I use vinyl ester resin for vacuum infusion. Any solutions?

I have attached photos of brand new and used for 2 weeks mustang louvers





Thank you!
Attachments
20140930_125505.jpg (396 views, 669.00 KB)
20140930_125430.jpg (482 views, 642.00 KB)
20140930_125505.jpg (461 views, 669.00 KB)
20140930_125451.jpg (472 views, 537.00 KB)
20140930_142934.jpg (461 views, 469.00 KB)
Reply
Dravis
Dravis
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
A simple solution to this problem may well be to use polyester Gelcoat, instead of GC50 ??..It's cheaper as well .. And highly UV resistant.

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)