When you post cure a mold, do you need to take the part out of it first or do you post cure with the part still in it?  For example, I'm molding hoods and I want to leave the hood in the mold so once it cures I can mold the other side?  So do I leave the hood in the mold, post cure and then mold the other side or do I remove the hood, post cure, put the hood back in, mold that then post cure again while the part is sandwiched inside?  Or will I need to split the molds, remove the part, and then post cure the newly molded half seperately?

I hope what I'm asking makes sense.
Replies
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
It always helps to post-cure with the part still in the mould. 

That said, you don't normally separately post-cure each part of a split mould. Make the entire mould first, then post-cure before demoulding. 
gabbett1
gabbett1
Forum Guru (72 reputation)Forum Guru (72 reputation)Forum Guru (72 reputation)Forum Guru (72 reputation)Forum Guru (72 reputation)Forum Guru (72 reputation)Forum Guru (72 reputation)Forum Guru (72 reputation)Forum Guru (72 reputation)
Group: Forum Members
Posts: 6, Visits: 219
Ok, I wondered about that.  How much time do you have to post cure once a mold goes through the ambient temp cure process?  Reason I ask is that if I'm molding a front and back of a part, it could be 24 hours+ that the first half would have already been molded and cured before the post cure process would start with both halves molded.
Edited 11 Years Ago by gabbett1
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search