Buying a decent size vacuum chamber costs upwards of £1000 but all we really need is some plastic tubing, thick plastic sheet to cap the ends, pvc hose and silicone.

The problem has always been how to get an airtight seal at the opening, well I found some airtight foam strips/sticky backed that were being sold to carpenters to hold down work with a vacuum, but the product was expensive and cut into thin strips Vacuum Workholding Product.  
So I trawled the suppliers database and found out the raw material was made in a town bordering my own.  Munsch & Co make all types of airtight foams and they can sell you a sheet as large as you need at a very cheap price. 

Ive got a 30cm x 30cm square metal baseboard, covered in airtight foam, with a hole drilled in the middle which is connected to a vacuum pump that id bought from carbon mods.  If i place any jar over the middle and turn the vacuum pump on the pressure pulls the jar into the foam creating an airtight seal.  The beauty of this system is you can change the size of belljar to suit your job, a coffee jar is good for degassing and I use a big clear plastic tube for larger jobs.

Pics coming soon...
Reply
ant...
ant...
Supreme Being (133 reputation)Supreme Being (133 reputation)Supreme Being (133 reputation)Supreme Being (133 reputation)Supreme Being (133 reputation)Supreme Being (133 reputation)Supreme Being (133 reputation)Supreme Being (133 reputation)Supreme Being (133 reputation)
Group: Forum Members
Posts: 17, Visits: 92
^ Perspex top - thats what made yours work better.  I tried using the lid, I bought 2 lots of rubber seal, used silicone but never got it to work Blink
Edited 13 Years Ago by ant...
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search