Hello guys!!

Wheb my fried arrived today at my home for me to do some engine work.... we found (in a bad way)  out its sitting pretty low+
when entering my garage he scratched his left side skirt.. 

I am pretty sure i could sand+polish ... But some of them are rather rough...
Any ideas ?
http://www.talkcomposites.com/Uploads/Images/aa8e2759-0e7c-49eb-a94c-6d60.JPG



http://www.talkcomposites.com/Uploads/Images/343d5699-faf3-4282-be06-64cf.JPG


http://www.talkcomposites.com/Uploads/Images/a16e82f2-9327-46d1-a209-27dc.JPG
Edited 12 Years Ago by Neutronetix
Reply
Neutronetix
Neutronetix
Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)
Group: Forum Members
Posts: 3, Visits: 58
OK, thanks for the information.

First i am gonna take my chances in repairing...
And if it does not turn out nicely i wil make it as smooth as possible and make a entire new mold for the part.ure

I have something to add:

Since i never had a broken piece of carbon fibre to take a look at i really have no idea ....
But the cured resin appaers to be really thick ... 
I am thinking its the way for the manufacturer to make parts ( wich dont need to be as strong ) 
cheaper to produce?



here is a other picture, mayby its more clear for you guys ?


http://www.talkcomposites.com/Uploads/Images/dad2e111-897d-4757-b962-bb1e.JPG
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search