Pattern coat gloss, applying an extra coat?


Author
Message
Bonobo
Bonobo
Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)
Group: Forum Members
Posts: 85, Visits: 1.2K
Any issues with applying an extra coat to fully cured pattern coat hi gloss? I'm flatting to 400 grit and have a few break through's.
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Should be fine, just make sure you prep the surface well. Not sure if the Pattern Coat range is thixotropic enough to avoid fisheyes, but they are a pain to rub out when they do happen so best to make sure they don't. Clean surface at a minimum, possibly very quick scuff with some 120 grit as well. 