Carbon on plywood


Author
Message
panda
panda
Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)
Group: Forum Members
Posts: 47, Visits: 2.1K
I have been laminating 200g twill carbon onto 5mm plywood recently to make kayak footrests and vacing them using the EL2 epoxy and slow hardener.  Most of the time they come out perfectly and just what the customer wants but every so often the carbon does not bond to the wood in a corner.  I always make sure the wood and carbon are fully saturated and down properly but 1/10 this always happens to and is always on an edge at a corner.

Any help or ideas are welcome!

Reply
panda
panda
Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)
Group: Forum Members
Posts: 47, Visits: 2.1K
It's for sprint kayaks, most of the boat is made of composites which makes it a bit nicer to have carbon footrests as well!

www.pandakayaks.co.uk
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search