My rs4 doors arent like normal doors in that the bottom where the outer skin and the inner have a good break point. imagine the 2 parts of a hood and where they meet.  The outer skin wraps around the inner. Where would be the best place to break this for an outer and inner 2 part mold. How would you bond the 2 halves together in this area?

here are some pics of what I mean. they are in primer cause I fixed the dents in them. 