what am I doing wrong ? / is this possible?


Author
Message
robjohnson
robjohnson
Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)
Group: Forum Members
Posts: 10, Visits: 55
hi, is it possible to make these panels without an infusion kit? thanks 
Attachments
door card.JPG (519 views, 1.00 MB)
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Yes definitely. Wet lay, like all composite processes, always takes a bit of practice.

From the pictures, that panel looks a little resin starved.