Hi all
Just thought i would share this with you, i have two of the smaller EC vac pumps and both have given me good service but i had noticed one was becoming very slow at pulling full vacuum. I decided to change the oil as it was due but noticed no difference in performance so i dismantled and inspected the vane pump and checked the valves and all was good. Whilst i had the pump body removed i opened the air valve and tried to blow through the valve only to find that air did NOT travel through it easily. I removed the valve to find a small gauze filter  partially blocked with resin, i removed the blockage and now the pump is as good as new. I do not recall the pump having sucked in any resin as i use catch pots but at some point it clearly had ingested a small amount.
Chris 
carbon fibre works ltd

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
Edited 11 Years Ago by carbonfibreworks
Replies
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
carbonfibreworks (11/06/2014)
Hi all
Just thought i would share this with you, i have two of the smaller EC vac pumps and both have given me good service but i had noticed one was becoming very slow at pulling full vacuum. I decided to change the oil as it was due but noticed no difference in performance so i dismantled and inspected the vane pump and checked the valves and all was good. Whilst i had the pump body removed i opened the air valve and tried to blow through the valve only to find that air did NOT travel through it easily. I removed the valve to find a small gauze filter  partially blocked with resin, i removed the blockage and now the pump is as good as new. I do not recall the pump having sucked in any resin as i use catch pots but at some point it clearly had ingested a small amount.
Chris 
carbon fibre works ltd



Cheers Chris great info there. One of my pumps is noticeably slow, well slower to pull vac will give what you suggest a go when I get chance. Like you I have to say the pumps from EC have been faultless and they get used on almost a daily basis. The one with the issue is nearly two years old. Bloody good value for money in my book.Smile

Warren

Carbon Copies Ltd
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
very happy about the pump as well! 
Warren, could you take some pictures while opening and cleaning the pump? I would like to do the same if you get some good results but I have no clue where to start or what to clean exactly Smile 

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
matthieutje65 (13/06/2014)
very happy about the pump as well! 
Warren, could you take some pictures while opening and cleaning the pump? I would like to do the same if you get some good results but I have no clue where to start or what to clean exactly Smile 



Will do. Hopefully it will go well and be a "how to service a vac pump" and not a "how NOT to service a vac pump" tutorial.w00t

Warren

Carbon Copies Ltd
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search