Hi, my name is nick, i m rebuilding my RD04 , 1990 , africa twin. i want to build a carbon fiber fuel tank using the original as model , maybe increasing fuel capacity . it is a large tank, 24l , so i m thinking about reinforcements , wave breakers.. I appreciate any advice regarding methods of construction , moulds, bonding external with 'tunnel' ...inserting threaded bushes for fuel taps.. etc.  I have a two stage vacuum pump Robinair , 71 / min, is it any good? Thanks 
Attachments
2014-05-25 11.10.30.jpg (409 views, 412.00 KB)
2014-05-25 11.12.12.jpg (421 views, 548.00 KB)
Edited 11 Years Ago by nick
brainfart
brainfart
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 198, Visits: 1.4K
Since nobody has replied so far I'll bite.

Vacuum pump is perfect (if it is in working condition).

Here's a link to get you started:

http://www.bayarearidersforum.com/forums/showthread.php?threadid=145975

I have a few issues with this built, (like don't know why he didn't use twill for the outer layer...), but then again he built a tank and I didn't.
morepower
morepower
Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)
Group: Forum Members
Posts: 242, Visits: 1.2K
Good luck with the project... 
nick
nick
Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)
Group: Forum Members
Posts: 2, Visits: 20
thanks, a split mould was in my mind too,, for the out part. the ' tunnel' is not so visible  but is full of holes ; africa tank have two fuel taps and indicators. my next step will be to talk to the guys on the staff to decide a list of materials and tools. 
brainfart
brainfart
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 198, Visits: 1.4K
Some things to consider:
Is a homemade tank street-legal? Todays fuel contain ethanol, which attacks many epoxy resins. Tank will need some kevlar if you drop the bike.
morepower
morepower
Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)
Group: Forum Members
Posts: 242, Visits: 1.2K
Making a tank is not too hard once you have figured out the moulding of it..
Legalities seem to be a none issue most places but it is worth checking, if you plan to sell them. 
Inserts for fuel taps and filler caps are not hard or expensive to source and I use normal woodworking T Nuts. 
Materials? Carbon for the inner and outer layers I would not use Kevlar personally I would use Diolen as it is a better material for abrasion compared to the more ballistic resistant Kevlar. Resin to seal against ethanol needs to be a Phenol Novolac resin. You can use it to make the tank fully or as a sealant. I do the latter as I make mine from Pre-preg carbon. 

Here are some photos.. I have made a tank only this week but had to modify one from my full monocoque seat/tank unit. I cut it down roughly to allow me to make the tank outer and trim it down and tidy up edges when I install the tank base. 

Sealed with a phenol novolac resin
Now assembly... But this is from when I assembled the full monocoque