Edwin
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 8,
Visits: 42
hi guys im new on this, i never try it before, i was wondering can i just spray the 3m super 77
direct on the mold to avoid the CF to moving, i'm using vacuum infusion way, its kinda hard and i take about 3 hour
just to prepare the CF, to be wrap on bagging film. OMG im so nOOB!
what i want to know is
1- if i spay it direct on the mold and then i put the 1st layer of Carbon
is it gonna stick on the mold by the time i want to demold it?
2- is it gonna effect my finishing i mean it gonna left me stain on the curing resin?
3 - or other effec?
pls help me for those who have experience on this.
Reply
Like
3
Reply
ajb100
ajb100
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 346,
Visits: 4.4K
I haven't used the 3m product, but use similar sprays.
You can apply directly to the mould and the fabric will stick fine. Due to your release agent, it will not stick when you come to de mould
As for the residue, the aerofix stuff I use does leave a bit of a pattern if used too heavily, but it your not using a gel coat, it polishes right off. Would have thought it would be the same as the 3m stuff
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
3M super 77 spray on the mold to avoid cp moving
Edwin
-
11 Years Ago
I haven't used the 3m product, but use similar sprays. You can apply directly to the mould and the...
ajb100
-
11 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search