Hello to everyones!

What are the techniques to make composite fiber sheets? I would like to obtain a good surface finish with excellent mechanical performance! 
I have 20ton hydraulic press (60x60cm enough for me) with heated plates (max. 250°C), it's useful?



Thank you!!
Reply
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
I have an old glass patio door I use for my flat sheets! Just vacuum on that at it gives a perfect finish