Hello all

Planning my first project.. I have included some photosbelow of the part to be replicated. Having lurked for a while I was hoping todraw on some experience here.. i have the large mould & high temp laminatekit from EC....

Mould construction

  • Would you build up the sides of the mould tomake the shape a complete ‘bowl’ and trim after, or using clay, construct anedge/flange following the contours of the shape..

Layup

  • ·        I had planned in the first instance to followthe wet lay technique shown on the video. What would be the most pleasing tothe eye to lay the fabric.. i planned to use two pieces of fabric due to theshape, firstly cap the top of the cowing using a circular-ish piece and use aseparate piece of cloth to cover the sides.
  • ·        Are there any issues with overlapping the cloth ..any special considerations in doing this,, will it look nasty.
  • ·        How many layers of fabric would typically beused to achieve the same thickness at the sample in the photos. this will besubject to vibration and heat
  • ·        Can i let each layer cure fully before addingthe next or should it all be laid in one sitting
  • ·        Can something of this deep bowl shape be doneusing a Vacuum bagging. Is there anything on the web showing this type of shapebeing made this way.. all i have found is flat or shallow panels.

Thanks

http://i834.photobucket.com/albums/zz270/unavailable404/IMG_0381.jpg

http://i834.photobucket.com/albums/zz270/unavailable404/IMG_0380.jpg

http://i834.photobucket.com/albums/zz270/unavailable404/IMG_0385.jpg


Reply
Matthieu Libeert
Matthieu Libeert
Supreme Being (10K reputation)Supreme Being (10K reputation)Supreme Being (10K reputation)Supreme Being (10K reputation)Supreme Being (10K reputation)Supreme Being (10K reputation)Supreme Being (10K reputation)Supreme Being (10K reputation)Supreme Being (10K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K

Can something of this deep bowl shape be doneusing a Vacuum bagging. Is there anything on the web showing this type of shapebeing made this way.. all i have found is flat or shallow panels.
________________________________________________________________________________________________

I have made a video tutorial on a "similar piece"...
http://www.youtube.com/watch?v=0tosbURJY0Q

and this one with carbon fiber http://www.youtube.com/watch?v=dn_xmEIiGQU&feature=context&context=C469f61fVDvjVQa1PpcFOPA_6CVAP8TkPgvS0r4v7CJrT1e6EGrEg= 

I will do another tutorial on a Fieldhockey goalie helmet laying Carbonfiber and Kevlar using vacuum infusion on the mould you see here
http://www.talkcomposites.com/Uploads/Images/9ac2b548-35b2-486f-874f-5cdf.jpg


I will do this in a few weeks because I'm going to San Francisco for 2week, leaving tomorrow...
If interested you can also see the making of the mould with flanges and so on
http://www.youtube.com/watch?v=CS3s2PqDXOc&feature=plcp&context=C469f61fVDvjVQa1PpcFOPA_6CVAP8TkPgvS0r4v7CJrT1e6EGrEg%3D

I hope to be able to help you in a few weeks Wink

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




Edited 14 Years Ago by matthieutje65
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search