Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
if you're not in a hurry you could leave the plugs to season in a warm place for as long as possible, ideally a few months!!! That would get most the styrene out then you can pay someone to 2k coat over the top which should seal it ok and youll get away with it.
Worst case you could oven bake it to drive out the solvents but its not garunteed.
With hindsight, 2k is the better option in the future.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|