Hi there, i'm looking to form a plug for a new painted engine cover. I'm proposing to use cross section templates taken from the attached cad file, copied and cut out of 50mm celotex or kingspan insulation. I have used this method previously and once sanded to shape, covered it in car body filler. This was successful, however the skin formed over the foam plug was brittle. I'd like to be able to use a spray or paint finish that i can apply directly to the foam and flat down, or i need to skin the foam with a layer of glass fibre prior to building up coats of primer filler? If i skin the foam with glass fibre, which materials do i need to use and how much depth of construction should i allow for when cutting the foam section in order to ensure my finished plug will end up the desired size. Any advice or direction to any previous posts that cover this topic would be really useful. (The green area, as shown on the attached, I'm proposing to form out of the foam, with the pink constructed in MDF, is this a good idea or should i do it all in the foam ?). This is all for a one off item.
Attachments
image002.jpg (906 views, 59.00 KB)
Reply
ChrisR
ChrisR
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
yes you can (and I have a number of times) celotex tends to ball and grab when sanding, it's reasonably stable if supported correctly and i believe it is unreactive to most resins (although I have only used epoxy on it myself so best to check)

I've always glassed the plug then sanded & finished, you just have to make the foam part a little smaller to allow for the glass thickness
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search