Group: Forum Members
Posts: 454,
Visits: 2.5K
|
man i putted near my heating thing for couple minutes resin started to go like bubbles so definitely overheated. one part cured for no tacky surface 3 days unreal. i tryed esterday to lay one layer when was plus 15 so lets see today. my main scary thing from me is i hope carbon not got condensate before i layed it.
|