Group: Forum Members
Posts: 363,
Visits: 3K
|
Hi, not sure on the exact properties but pretty much anything is going to have higher properties than CSM glass.
Cores are fine but I wouldn't use them all over, just up the back. Wherever you have a mounting point I'd put a few extra layers and no core so the laminate won't crush when you bolt through and it will give a more uniform bearing surface for the bolt.
My old sparco glass seats are about 4mm thk CSM if that helps and thicken up wherever there's a mounting point.
|