By kursatdurmaz - 2/28/2014 7:30:28 PM

Hi everybody!

I am a newbie who am a team member of univetsity solar car project. I'm responsible for composite part production. We are planning to make inner stiff chasis from sandwich panels(closed cell pvc- 2x2 twill carbon fibre sandwich).  We would like to use wooden mould. However I have no experience about  wooden mould surface finishing. Is gelcoat coating enough basically or have I use different finishing materials?

Regards.

Kürsat.
By kursatdurmaz - 3/3/2014 8:33:16 PM

omg Smile) thats really fantastic and make good sense!