1. 42.7mm closest tube has a 40.9 OD. This would leave a 0.9mm joint gap all the way around.
2. 33.1mm closest tube has a 31.3 OD. This would leave a 0.9mm joint gap all the way around.
3. 30mm closest tube has a 29.3 OD. This would leave a 0.35mm joint gap all the way around.
So I have a few question about resolving the difference.
1. What is the recommended gap/joint space when sleeving carbon tubes with metal?
2. Can Easy Composites supply custom tubing at the these OD 30/33.1/42.7mm suitable for bonding the to the OD?
3. Please can you recommend the best adhesive?
Thank you