By udog - 2/20/2014 8:41:36 AM
Hi Id like to know what are the main differences between using a venturi vacuum system and a pump sistem. Purchasing a venturi one seems cheaper(already have a good compresor),but Id like to know what is the downside if there is,and its limits. We are focusing on small bycicle parts,no infusion. Thanks in advance.
|
By udog - 2/21/2014 9:00:47 AM
Thanks fo the reply rObsk1
So it works,but,thinking of it twice and taking in account other replies in another section of the forum,it might be wise to get a pump,just in case one day we want to go for bigger parts etc...sounds its worth it in long term.
"sound like an air rifle firing everytime vacuum drops"
Know what you mean....get that feeling once in a while
Thanks for the info!
|
|