By Yvesdlf - 2/19/2014 6:50:26 PM

I'm planning to apply skinning on lexan, will the base coat be ok, would there be any sort of reaction that can distort the lexan or with the resin?
By Warren (Staff) - 2/21/2014 9:20:24 AM

Epoxy should bond no problem.  We always recommend keying the surface first.