Thanks Matthieu!
Actually i have watched your video many times, really good instructions! So far i have repaired one blade and two shafts. Blade repair went quite well, shafts looked nice but didn't work and now both are broken again. My intension is to practice with ice hockey sticks and when i have enough experience i will try to repair bike frames.