By carbonfibreworks - 1/29/2014 10:17:18 PM

Made using infusion with carbon/soric and epoxy resin with a nice gloss straight from the mould, I used pro finish for the V weave and it was still complex due to the compound curve of the panel. 



By FLD - 1/31/2014 7:41:26 AM

Looks awesome!  Top work there.