Is this a recommended/accurate way to cut foam?

I am attempting to create a diffuser. This piece would act as the core unless it is suggested to use a different material.

Any info would be appreciated, Thanks!
By ajb100 - 1/13/2014 3:00:32 PM

Hot wire cutter would be fine, but I just use a Stanley knife, hold it at a low angle so it cuts progressively and then snap it apart